n) assembling the first arrays into the second array;
o) assembling the second arrays into the EESU final assembly.
2. The method of claim 1 wherein a second coating of glass is provided on to the double-coated composition-
modified barium titanate powder being in contact with the nickel electrodes and having an applied working
voltage of 3500 V across the parallel electrodes.
3. The method of claim 1 wherein a dielectric voltage breakdown strength of 5.0 × 106 V/cm was achieved across
the electrodes of the components.
4. The method of claim 1 wherein the method provides an ease of manufacturing due to the softening temperature
of the calcium magnesium aluminosilicate glass allowing the relatively low hot-isostatic-pressing temperatures
of 700OC which in turn provides a void-free ceramic body.
5. The method of claim 1 wherein the method provides an ease of fabrication due to the softening temperature of
the calcium magnesium aluminosilicate glass allowing the relatively low hot-isostatic-pressing temperatures of
700OC which in turn allows the use of nickel for the conduction-path electrodes rather than expensive platinum,
palladium, or palladium-silver alloy.
6. The method of claim 1 wherein the method provides an ease of fabrication due to the softening temperature of
the calcium magnesium aluminosilicate lass allowing the relatively low hot-isostatic-pressing temperatures of
700OC, which feature along with the coating method provided a uniform-thickness shell of the calcium
magnesium aluminosilicate glass and in turn provides hot-isostatic-pressed double-coated composition-
modified barium titanate high-relative-permittivity layers that are uniform and homogeneous in microstructure.
7. The method of claim 1 wherein the method provides the double coating of the basis particles of the
composition-modified barium titanate powder thereby reducing the leakage and ageing of this material by an
order of magnitude of the specification of this basis material, thus reducing the discharge rate to 0.1% per 30
days.
8. The method of claim 1 wherein the method provides a double coating of the composition-modified barium
titanate powder, the hot-isostatic-pressing process, the high-density solder-bump packaging, and along with
the double-layered array configuration stored 52,220 W·h of electrical energy in a 2005 inches3 container.
9. The method of claim 1 wherein the method provides materials used: water-soluble precursors of barium (Ba),
calcium (Ca), titanium (Ti), zirconium (Zr), manganese (Mn), yttrium (Y), neodymium (Nd), forming the
composition-modified barium titanate powder, and the metals: nickel (Ni), and copper (Cu), which are not
explosive, corrosive, or hazardous.
10. The method of claim 1 wherein the method provides an EESU that is not explosive, corrosive, or hazardous
and therefore is a safe product when used in electrical vehicles, which include bicycles, tractors, buses, cars,
or any device used for transportation or to perform work.
11. The method of claim 1 wherein the method provides an EESU which can store electrical energy generated
from solar voltaic cells or other alternative sources for residential, commercial, or industrial applications.
12. The method of claim 1 wherein the method provides an EESU which can store electrical energy from the
present utility grid during the night when the demand for electrical power is low and then deliver the electrical
energy during the peak power demand times and thus provide an effective power averaging function.
13. The method of claim 1 wherein the method provides a double coating of the composition-modified barium
titanate powder and a hot-isostatic-pressing process which together assists in allowing an applied voltage of
3500 V to a dielectric thickness of 12.76×10-6 m to be achieved.
14. The method of claim 1 wherein the method provides a EESU which when fully discharged and recharged, the
EESU's initial specifications are not degraded.
15. The method of claim 1 wherein the method provides a EESU which can be safely charged to 3500 V and store
at least 52.22 kW·h of electrical energy.
16. The method of claim 1 wherein the method provides a EESU at has a total capacitance of at least 31 F.
Editorial commentary and evidence checks for this source
Check definitions, measurements and the difference between a model, a reported simulation and independently reproduced evidence. Spiritual or speculative interpretations do not become physical or clinical findings through notation.
A Practical Guide to Free-Energy Devices — Patrick J. Kelly — evidence guide
A large technical compilation mixes ordinary electrical mechanisms with unvalidated excess-energy claims. Require complete energy accounting, independent replication and safe experimental design.
An archive is a starting point, not an automatic truth certificate. A large technical compilation mixes ordinary electrical mechanisms with unvalidated excess-energy claims. Require complete energy accounting, independent replication and safe experimental design.
Full commentary and investigation questionsThe source text is preserved as attributed material; commentary does not rewrite an allegation into a verified finding.